portada Evaluation of Novel Metalorganic Precursors for Atomic Layer Deposition of Nickel-Based Thin Films (en Inglés)
Formato
Libro Físico
Editorial
Idioma
Inglés
N° páginas
132
Encuadernación
Tapa Blanda
ISBN13
9783668112254

Evaluation of Novel Metalorganic Precursors for Atomic Layer Deposition of Nickel-Based Thin Films (en Inglés)

Varun Sharma (Autor) · Grin Verlag · Tapa Blanda

Evaluation of Novel Metalorganic Precursors for Atomic Layer Deposition of Nickel-Based Thin Films (en Inglés) - Varun Sharma

Libro Nuevo Importado
Envío: 18 a 22 días háb.
63,37 €57,04 €
-10%
Libro Nuevo

Quedan 10 unidades

57,04 €
Llega entre el 20 Ago y el 28 Ago a Provincia de Madrid. Seleccionar ubicación

Reseña del libro "Evaluation of Novel Metalorganic Precursors for Atomic Layer Deposition of Nickel-Based Thin Films (en Inglés)"

Master's Thesis from the year 2015 in the subject Physics - Electrodynamics, grade: 1.0, Dresden Technical University (Faculty of Electrical and Computer Engineering/Institute of Semiconductors and Microsystems), course: Nanoelectronic Systems, language: English, abstract: Nickel and nickel(II) oxide are widely used in advanced electronic devices. In microelectronic industry, nickel is used to form nickel silicide. The nickel mono-silicide (NiSi) has emerged as an excellent material of choice for source-drain contact applications below 45 nm node CMOS technology. As compared to other silicides used for the contact applications, NiSi is preferred because of its low resistivity, low contact resistance, relatively low formation temperature and low silicon consumption. Nickel is used in nickel-based rechargeable batteries and ferromagnetic random access memories (RAMs). Nickel(II) oxide is utilized as transistor gate-oxide and oxide in resistive RAMs. Atomic Layer Deposition (ALD) is a special type of Chemical Vapor Deposition (CVD) technique, that is used to deposit very smooth as well as homogeneous thin films with excellent conformality even at high aspect ratios. In spite of huge number of practical applications of nickel and nickel(II) oxide, a few nickel precursors are available for thermal based ALD. Moreover, these precursors have resulted in poor film qualities and the process properties were also limited. Therefore in this master thesis, the properties of various novel nickel precursors had to be evaluated. All novel precursors are heteroleptic (different types of ligands) complexes and were specially designed by the manufacturer for thermal based ALD of pure nickel with hydrogen as a co-reactant. In order to evaluate the novel precursors, a new methodology was designed to test small amounts (down to 2 g) of precursors in a very time efficient way. This methodology includes: TGA/DTA curve analyses of the precursors, thermal stability tests in which the pre

Opiniones del libro

Preguntas frecuentes sobre el libro

Todos los libros de nuestro catálogo son Originales.
El libro está escrito en Inglés.
La encuadernación de esta edición es Tapa Blanda.